Alginate was originally developed in the 1930s and has become the most commonly used impression material worldwide.

Material Properties

ANSI/ADA Specifications 18-1992

  • Compressive Strain - between 5-20%
  • Compressive Strength ≥ 0.35MPa
  • Elastic Recovery ≥ 95%
  • Not Specified
    • Tear Strength 100-300 J/m2